Jump to content

Recommended Posts

Posted

What aluminum alloy does Mooney use on the wing skins and how thick is it? Are the formed aluminum pieces such as gear doors etc a different alloy?

Posted

Per the SMM, the ribs, skins, and doublers are 2024 T3, T4, or T42 aluminum alloy.  I cannot find data, but the doors feel like 2024-t3. as well.


The fuel tank area is .050 and .040 in the fuel tank area, then .032 and then .025 in the wing tip area.   photo enclosed.

post-6498-13468141054142_thumb.jpg

Posted

I'm pretty sure Mooney purchases the 2024 in the T0 or annealed condition for the gear doors.  They form it 1st and then send it out to be heat treated and aged to the T4 condition.  It doesn't form that well in the T3 or T4 condition and is prone to crack if complex forming is done in that condition.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

We have placed cookies on your device to help make this website better. You can adjust your cookie settings, otherwise we'll assume you're okay to continue.